Jump to content

File:Steamer process develop fig1.png

From LabAdviser
Revision as of 12:19, 29 September 2014 by Paphol (talk | contribs) (The average silicon dioxide thickness and the percent of film non-uniformity over the boat variation with process time, steamer flow rate and temperature.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Steamer_process_develop_fig1.png (527 × 324 pixels, file size: 17 KB, MIME type: image/png)

The average silicon dioxide thickness and the percent of film non-uniformity over the boat variation with process time, steamer flow rate and temperature.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:19, 29 September 2014Thumbnail for version as of 12:19, 29 September 2014527 × 324 (17 KB)Paphol (talk | contribs)The average silicon dioxide thickness and the percent of film non-uniformity over the boat variation with process time, steamer flow rate and temperature.