CSAR


AllResist SX 6200/2 spinning on Manual Spinner LabSpin A-5, TIGRE, 09-04-2014
Spin Speed [rpm] Acceleration [1/s2] Spin Time [s] Thickness [nm] St Dev
2000 4000 60
3000 4000 60
4000 4000 60
5000 4000 60
6000 4000 60
7000 4000 60