Deposition of Germanium
Germanium can be deposited by thermal evaporation.
| Thermal evaporation (Wordentec) | E-beam evaporation (Physimeca) | |
|---|---|---|
| General description | Thermal deposition of Ge | E-beam deposition of Ge |
| Pre-clean | RF Ar clean | - |
| Layer thickness | 10Å to about 2000Å | 10Å to about 3000Å |
| Deposition rate | From 0.4 Å/s up to about ~2Å/s | From 5 Å/s up to 10/s |
| Batch size |
|
|
| Allowed substrates |
|
|
| Allowed materials |
|
|
| Comment | Recommended for unexposed e-beam resist | . |