Specific Process Knowledge/Thin film deposition/Deposition of NiV
Appearance
Feedback to this page: click here
Nickel Vanadium can be deposited by sputter evaporation. In the chart below you can compare the different deposition equipment.
| Sputter deposition (PVD co-sputter/evaporation) | Sputter deposition (Sputter-System Lesker) | |
|---|---|---|
| General description | Sputter deposition of NiV | Sputter deposition of NiV |
| Pre-clean | RF Ar clean | RF Ar clean |
| Layer thickness | About 10Å to 4000Å | About 10Å to 5000Å |
| Deposition rate | Depending on process parameters. | Depending on process parameters. |
| Batch size |
|
|
| Allowed substrates |
|
|
| Allowed materials |
|
|
| Comment | Sputter target with NiV composition: Ni/V 93/7% | Sputter target with NiV composition: Ni/V 93/7% |