Platinum deposition
Platinum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | Sputter deposition (Lesker) | |
|---|---|---|---|
| General description | E-beam deposition of Pt | E-beam deposition of Pt | Sputter deposition of Pt |
| Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 5000Å* | 10Å to 5000Å* | 10Å to 5000Å |
| Deposition rate | 2Å/s to 15Å/s | 10Å/s to 15Å/s | ? Å/s to ? Å/s |
| Batch size |
|
|
|
| Allowed materials |
|
|
|
| Comment |
* For thicknesses above 200 nm permission is required from Thin Film group.