TPT Wire Bonder
The TPT Wire Bonder is a new machine bought i 2007. Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT-H05 is a manuel wire bonder.
Please be aware that the bonder only is operated by Danchip personal.
Wedge Bonding
- Gold wire 25 µm wire.
- Aluminium wire 25 µm wire.
- Min. bonding area 200 µm.
Ball Bonding
Ball bonding gives free choice of bonding direction. First bond forms a small ball and second bond is a wedge bond.
- Gold only 25 µm wire.
- Min. bonding pad 300 µm.
- Sample withstand heating to 120 oC.