Gold can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | Sputter (Lesker) | Sputter coater Hummer | Sputter coater Balzer | |
|---|---|---|---|---|---|
| Batch size |
|
|
|
|
|
| Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean | ||
| Layer thickness | 10 Å to 5000Å* | 10 Å to 5000Å* | 10 Å to | ||
| Deposition rate | 2 Å/s to 10 Å/s | 1 Å/s to 10 Å/s | Not measured | Not measured | |
| Allowed materials |
|
|
|
. | . |
| Comment | For thicknesses above 200 nm
permission is required |
For thicknesses above 200 nm
permission is required |
Used to gold sputter coating of
samples mainly before SEM characterization |
Used to gold sputter coating of
samples mainly before SEM characterization |
* For thicknesses above 200 nm permission from ThinFilm group (thinfilm@danchip.dtu.dk) is required.
Adhesion of Au on Si
Studies of Au deposition processes
Roughness of Au layers - Roughness of Au layers deposited with different equipment and settings