Specific Process Knowledge/Wafer cleaning
Appearance
Feedback to this page: click here
Clean with:
- RCA - Two step process to remove organics and metals
- 7-up & Piranha - Removes organics and alkali ions
- 5% HF - Removing native oxide
- IMEC - Cleaning before fusion bonding
- Soap Sonic - Cleaning of "dirty" wafers when entering the cleanroom
Section under construction
Comparison of Wafer Cleaning Methods
| RCA | 7-up & Piranha | 5% HF | IMEC | Soap Sonic | |
|---|---|---|---|---|---|
| Generel description | Two step process to remove organics and metals | Removes organics and alkali ions | Removing native oxide | Cleaning before wafer bonding | Removing dust and particles |
| Purpose | Mandatory prior furnace processes | When needed and always after KOH etch and Nitride etch in Phosphoric acid | Optional with RCA cleaning | Cleaning before wafer bonding | Cleaning very dirty items that enters the cleanroom. Should be followed by a piranha clean. |
| Substrate size |
|
|
|
|
|
| Allowed materials |
|
|
|
|
|