Specific Process Knowledge/Characterization/AFM: Atomic Force Microscopy

From LabAdviser

Nanoman

 
Nanoman: positioned in cleanroom 4 - glass cage no. 4

The AFM: Nanoman is a product of Veeco Instruments. AFM stands for Atomic Force Microscope which is a scanning probe microscope where a sharp probe is scanned across a surface either in contact mode or tapping mode. The outcome is a topographic plot of the surface. It has a lateral solution of about 1 nm and a vertical resolution of less than 1 Å which makes it very suitable for topographic characterization in the nanometer regime. The limiting factor however is often the size of the probe in use. The tip radius of curvature (ROC) can be from 2 nm up to more than 20 nm depending on the chosen probe. The half cone angle of the tip can be vary from less than 3o to over 25o giving problems resolving high aspect ratio structures.

To get some product information from the vendor take a look at Veeco's homepage [1]

A rough overview of the performance of the AFM: Nanoman

Purpose Profiler for measuring micro structures.
  • Single point profiles
  • Wafer mapping
  • Stress measurements by measuring wafer bow
  • Surface roughness on a line scan
Performance Scan range xy

Line scan x: 50 µm to 200 mm

. Scan range z

50 Å to 262 µm

. Resolution xy

down to 0.067 µm

. Resolution z

1Å, 10Å or 20Å

. Max. scan depth as a function of trench width W

1.2(W[µm]-5µm)

Hardware settings Tip radius
  • 5 µm 45o cone
Substrates Substrate size
  • up to 8"
. Substrate material allowed
  • In principle all materials