Specific Process Knowledge/Characterization/Optical microscope

From LabAdviser
Zeiss (RR2) Leica (RR3) Leitz (RR4 Glassroom1) Zeiss (RR4 Glassroom1) Zeiss (RR4) Nikon (K10 yellow room)
Magnification 25,50,100,

200,500x

50,100,200,

500,1000x

25,50,100,

200,500x

50,100,200,

500,1000x

25,50,100,

200,500x

50,100,200,

500,1000x

Bright field yes yes yes yes yes yes
Dark field yes yes yes yes yes yes
Polarizer yes no no yes yes no
Episcopic light (reflected light) yes yes yes yes yes yes
Diascopic light (transmitted light) no yes yes no no yes
View with eye yes yes yes yes yes yes
View on screen no yes yes yes no yes
Measurement option no no yes yes no yes