Upload log
Appearance
Below is a list of the most recent file uploads. See the gallery of new files for a more visual overview.
- 14:35, 30 July 2025 Eves talk contribs uploaded File:Eves Ta RT GiXRD rawta ft may 2025.png (File uploaded with MsUpload)
- 14:35, 30 July 2025 Eves talk contribs uploaded File:Eves Ta 500C XRR rawta ft may 2025.png (File uploaded with MsUpload)
- 14:35, 30 July 2025 Eves talk contribs uploaded File:Eves Ta 500C GiXRD rawta ft may 2025.png (File uploaded with MsUpload)
- 15:18, 28 July 2025 Prakus talk contribs uploaded a new version of File:SRN slowetch profilealong center.png (File uploaded with MsUpload)
- 15:15, 28 July 2025 Prakus talk contribs uploaded File:SRN slowetch profilealong center.png (File uploaded with MsUpload)
- 14:06, 28 July 2025 Prakus talk contribs uploaded File:SRN slowetch data 100%load.png (File uploaded with MsUpload)
- 11:41, 28 July 2025 Prakus talk contribs uploaded File:SRN etch rate uniformity nochambercondition.png (File uploaded with MsUpload)
- 10:46, 28 July 2025 Prakus talk contribs uploaded File:Slowetch2 100% loadSRN etchrate.png (File uploaded with MsUpload)
- 10:43, 28 July 2025 Prakus talk contribs uploaded File:Slowetch2 100% loadSRN.png (File uploaded with MsUpload)
- 10:29, 28 July 2025 Prakus talk contribs uploaded File:Slowetch2 data 100%load.png
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XRR NbN Ar10 N2 20 temp test 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XRR NbN Ar20 N2 16 temp test 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS survey NbN wafer9 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS survey NbN wafer4 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS survey NbN wafer3 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS O1s NbN wafer10 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS O1s NbN wafer9 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS O1s NbN wafer4 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS O1s NbN wafer3 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS Nb3d NbN wafer10 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS Nb3d NbN wafer9 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS Nb3d NbN wafer4 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS Nb3d NbN wafer3 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS N1s NbN wafer10 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS N1s NbN wafer9 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS N1s NbN wafer4 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS N1s NbN wafer3 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS composition NbN wafer10 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS composition NbN wafer9 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS composition NbN wafer4 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS composition NbN wafer3 500C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves XPS survey NbN wafer10 700C 20250724.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE uniformity wafer5 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer8 n 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer8 k 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer8 e2 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer8 e1 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer5 n 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer5 k 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer5 e2 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE optical function NbN wafer5 e1 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves SE uniformity wafer8 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves RSM 200 NbN PC3 Ar 20 N2 16 500C 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves RSM 113 NbN PC3 Ar 20 N2 16 500C 20250723 2.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves RSM 113 NbN PC3 Ar 20 N2 16 500C 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves HRXRD NbN PC3 Ar 20 N2 16 temp test 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves HRXRD NbN PC3 Ar 10 N2 20 temp test 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves HRXRD NbN PC3 700C flow test 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves HRXRD NbN PC3 600C flow test 20250723.png (File uploaded with MsUpload)
- 19:16, 25 July 2025 Eves talk contribs uploaded File:Eves HRXRD NbN PC3 500C flow test 20250723.png (File uploaded with MsUpload)