- 18:47, 7 February 2024 Eves talk contribs uploaded File:Eves Gd02Ce08O2 120W 3mTorr RT ArO2 50 2 1800s uniformity image 20231128.png (File uploaded with MsUpload)
- 17:36, 7 February 2024 Eves talk contribs uploaded File:Eves Au resistive thermal evporation image2 EVC5 20240207.png (File uploaded with MsUpload)
- 17:36, 7 February 2024 Eves talk contribs uploaded File:Eves Au resistive thermal evporation image1 EVC5 20240207.png (File uploaded with MsUpload)
- 17:36, 7 February 2024 Eves talk contribs uploaded File:Eves Au resistive thermal evporation rise soak box heater EVC5 20240207.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Ge onSi with 300nm SiO2 Thermal Evaporator 20231205 uniformity.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Ge onSi with 300nm SiO2 Thermal Evaporator 20231130 uniformity.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves Thermal Evaporation 8 inch wafer holder with adaptor 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves Ge refr index data 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves Ge evaporation rise soak settings 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves Ge evaporation from EVS8B005W 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves Ge evaporation 100nm Psi Delta 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves Ge abs coeff data 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves EVS20A015W 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Eves EVS8B005W 20240206.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:IMG 20240129 173018.jpg (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Image1.png (File uploaded with MsUpload)
- 17:08, 7 February 2024 Eves talk contribs uploaded File:Ge onSi with 300nm SiO2 Thermal Evaporator 20231220 uniformity.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Paphol SiO2 on Si evaporation 200C 5prO2 80nm uniformity 20231113 image.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation temperature 80nm sp RT 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation temperature 80nm sp 200C 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation rise soak 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation pressure 80nm sp RT 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation pressure 80nm sp 200C 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation power 80nm sp RT 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation power 80nm sp 200C 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation gas flow 80nm sp RT 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation gas flow 80nm sp 200C 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation dep rate 80nm sp RT 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation dep rate 80nm sp 200C 5 pr O2 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation 80nm sp 5 pr O2 Psi Delta 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Eves SiO2 evaporation 80nm sp 5 pr O2 optical functions 20240201.png (File uploaded with MsUpload)
- 16:46, 7 February 2024 Eves talk contribs uploaded File:Paphol SiO2 on Si evaporation RT 5prO2 80nm uniformity 20231109 image.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation rise soak 20240207.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation refr index 80nm sp 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation pressure 80nm sp RT 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation pressure 80nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation pressure 60nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation power 80nm sp RT 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation power 80nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation power 60nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation photo.jpg (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation gas flow 80nm sp RT 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation gas flow 80nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation gas flow 60nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation dep rate 80nm sp RT 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation dep rate 80nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation dep rate 60nm sp 200C 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 evaporation abs coefficient 80nm sp 5 pr O2 20240126.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 with 5prO2 and RT on Si with native oxide 80nm setpoint 20231103 uniformity.png (File uploaded with MsUpload)
- 16:35, 7 February 2024 Eves talk contribs uploaded File:Eves Al2O3 with 5prO2 and 200C heat on Si with native oxide 80nm setpoint 20231103 uniformity.png (File uploaded with MsUpload)