- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 SEM image2 20220727.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 SEM image1 20220727.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS valence 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS survey 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS O1s 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS C1s cluster etch 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS C1s cluster etch 2D 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS C1s 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma XPS Al2p 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma transmission 20220727.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma REELS 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma optical function 20220727.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma ISS 20220829.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma dep rate 20220728.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma 1000cycles uniformity 20220727.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 RT plasma 325cycles uniformity 20220727.png (MsUpload)
- 21:06, 29 August 2022 Eves talk contribs uploaded File:Eves ALD2 Al2O3 SEM image4 20220727.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC refractive index home 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC refractive index extended 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC home bias 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC Home 200W uniformity 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC Home 160W uniformity 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC Home 120W uniformity 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC extended bias 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC Ext 200W uniformity 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC Ext 160W uniformity 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC Ext 120W uniformity 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC deprate vs power 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC absorption coeff home 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC absorption coeff extended 20220802.png (MsUpload)
- 17:08, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si pDC thickness vs power 20220802.png (MsUpload)
- 14:31, 2 August 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF refractive index home 20220726 2.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si Extended position 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si Home position 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF refractive index home 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF refractive index extended 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF home bias 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Home 200W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Home 180W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Home 160W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Home 140W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Home 120W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF extended bias 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Ext 200W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Ext 180W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Ext 160W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Ext 140W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF Ext 120W uniformity 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF deprate vs power 20220726.png (MsUpload)
- 18:37, 27 July 2022 Eves talk contribs uploaded File:Eves PC3 Src1 Si RF absorption coeff home 20220726.png (MsUpload)