Upload log
Appearance
Below is a list of the most recent file uploads. See the gallery of new files for a more visual overview.
- 13:41, 9 February 2022 Paphol talk contribs uploaded File:2022-02-08 10-56-57 Wafer A2 150nm Rel.png
- 13:39, 9 February 2022 Paphol talk contribs uploaded File:2022-02-08 10-56-57 Wafer A2 150nm Abs.png
- 12:52, 9 February 2022 Paphol talk contribs uploaded File:2022-02-08 10-47-35 Wafer E1 117nm Rel.png
- 12:52, 9 February 2022 Paphol talk contribs uploaded File:2022-02-08 10-47-35 Wafer E1 117nm Abs.png
- 12:29, 9 February 2022 Paphol talk contribs uploaded File:E1 furnace.JPG
- 10:48, 25 January 2022 Jenk talk contribs uploaded File:TidyUP small.png
- 10:48, 25 January 2022 Jenk talk contribs uploaded File:MPOserver2 small.png
- 10:48, 25 January 2022 Jenk talk contribs uploaded File:MPOserver small.png
- 18:03, 20 January 2022 Eves talk contribs uploaded File:Eves Pt old lesker 250W 2021 short.png (MsUpload)
- 18:03, 20 January 2022 Eves talk contribs uploaded File:Eves Pt sample model 20220120.png (MsUpload)
- 17:26, 20 January 2022 Eves talk contribs uploaded File:Eves ZnO old Lesker SE uniformity pure Ar 20220120.png (MsUpload)
- 17:26, 20 January 2022 Eves talk contribs uploaded File:Eves ZnO old Lesker SE uniformity 10prO2 in Ar 20220120.png (MsUpload)
- 17:26, 20 January 2022 Eves talk contribs uploaded File:Eves ZnO old lesker 2021 with10prO2 short.png (MsUpload)
- 17:26, 20 January 2022 Eves talk contribs uploaded File:Eves ZnO old lesker 2021 noO2 short.png (MsUpload)
- 17:26, 20 January 2022 Eves talk contribs uploaded File:Eves ZnO absorption coefficient 20220120.png (MsUpload)
- 17:26, 20 January 2022 Eves talk contribs uploaded File:Eves ZnO refractive index 20220120.png (MsUpload)
- 16:55, 19 January 2022 Bghe talk contribs uploaded File:Monthly LabAdviser update 20220119.docx (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Si with and without native oxide XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Al2O3 general 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Al2O3 all XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Al2O3 8 nm XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Al2O3 6 nm XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Al2O3 4 nm XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves Al2O3 2 nm XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 general 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 all XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 8 nm XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 6 nm XRR 20211118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 4 nm XRR 202118 3.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 4 nm XRR 202118 2.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 4 nm XRR 202118.png (MsUpload)
- 00:13, 12 January 2022 Eves talk contribs uploaded File:Eves TiO2 2 nm XRR 20211118.png (MsUpload)
- 00:01, 12 January 2022 Eves talk contribs uploaded File:Eves Cr old lesker 220W 2021.png (MsUpload)
- 23:54, 11 January 2022 Eves talk contribs uploaded File:Eves Al old lesker 300W 2021.png (MsUpload)
- 23:52, 11 January 2022 Eves talk contribs uploaded File:Eves ZnO old lesker 2021.png (MsUpload)
- 23:48, 11 January 2022 Eves talk contribs uploaded File:Eves TiO2 old lesker 20W 2021.png (MsUpload)
- 23:46, 11 January 2022 Eves talk contribs uploaded File:Eves Ti old lesker 20W 2021.png (MsUpload)
- 23:46, 11 January 2022 Eves talk contribs uploaded File:Eves dep rate vs power Ti DC 3mTorr old Lesker 2021.png (MsUpload)
- 23:46, 11 January 2022 Eves talk contribs uploaded File:Eves Ti old lesker 250W 2021.png (MsUpload)
- 23:35, 11 January 2022 Eves talk contribs uploaded File:Eves Si RF old Lesker 20220110.png (MsUpload)
- 23:20, 11 January 2022 Eves talk contribs uploaded File:Eves Si RF sputtering dep rate 20211110.png (MsUpload)
- 23:20, 11 January 2022 Eves talk contribs uploaded a new version of File:Eves Si 120W 20211110.png (MsUpload)
- 23:20, 11 January 2022 Eves talk contribs uploaded File:Eves Si RF sputtering opt constants 20211110.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN uniformity 120W 20211111 3.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN uniformity 120W 20211111 2.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN uniformity 120W 20211111.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN uniformity 100W 20211111 3.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN uniformity 100W 20211111 2.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN uniformity 100W 20211111.png (MsUpload)
- 23:14, 11 January 2022 Eves talk contribs uploaded File:Eves SiN refr index 20211111.png (MsUpload)