- 17:09, 5 February 2013 Kn talk contribs uploaded File:8 1 metal on frontside.JPG
- 16:53, 5 February 2013 Kn talk contribs uploaded File:7 6 develop resist.JPG
- 16:48, 5 February 2013 Kn talk contribs uploaded File:7 2 spin resist.JPG
- 16:41, 5 February 2013 Kn talk contribs uploaded File:Color explanations.JPG
- 16:37, 5 February 2013 Kn talk contribs uploaded File:6 3 strip resist.JPG
- 16:36, 5 February 2013 Kn talk contribs uploaded File:6 1 oxide etch.JPG
- 16:33, 5 February 2013 Kn talk contribs uploaded File:5 4 development.JPG
- 16:28, 5 February 2013 Kn talk contribs uploaded File:5 2 resist spinning.JPG
- 16:25, 5 February 2013 Kn talk contribs uploaded File:4 4 oxidation.JPG
- 16:21, 5 February 2013 Kn talk contribs uploaded File:4 2 phosporus.JPG
- 16:14, 5 February 2013 Kn talk contribs uploaded File:3 3 resist strip.JPG
- 16:11, 5 February 2013 Kn talk contribs uploaded File:3 1 oxide etch.JPG
- 16:06, 5 February 2013 Kn talk contribs uploaded File:1 3 oxide.JPG
- 16:02, 5 February 2013 Kn talk contribs uploaded File:8 3 lift off.JPG
- 11:57, 5 February 2013 Kn talk contribs uploaded File:8 2 after metal before lift.JPG
- 10:14, 5 February 2013 Kn talk contribs uploaded File:Profile After lift off solar cell.JPG
- 11:27, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 3.jpg
- 11:24, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 2.gif
- 11:21, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 1.jpg
- 11:16, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 1.pdf (Unifromity of CNTS from BM)
- 11:16, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 2.pdf (Unifromity of CNTS from BM)
- 11:15, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 3.pdf (Unifromity of CNTS from BM)
- 09:47, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check.pdf (Carbon nanotubes from black magic. Uniformity across a wafer checked, and summarized in this file. )
- 16:45, 7 November 2012 Kn talk contribs uploaded File:CNTS uniformity check.pptx (Presenstation of a short study that was made to check the uniformity of CNTs grown in the Black magic system.)
- 12:17, 7 November 2012 Kn talk contribs uploaded File:W5 center.JPG (CNTs, wafer 5. Recipe "PECVD NH3.txt" 5 min growth.)
- 11:07, 7 November 2012 Kn talk contribs uploaded a new version of File:W6 center oposit.tif (CNTs wafer 6, recipe "PECVD NH3. txt")
- 11:06, 7 November 2012 Kn talk contribs uploaded File:W6 center oposit.tif (CNTs wafer 6, recipe "PECVD NH3.txt")
- 11:52, 6 November 2012 Kn talk contribs uploaded File:W3 center CNTs.JPG (Black Magic CNTs. recipe "PECVD NH3.txt" 10 min growth.)
- 11:48, 6 November 2012 Kn talk contribs uploaded File:W3 center CNTs.tif (Black Magic CNTs. recipe "PECVD NH3.txt" 10 min growth.)
- 13:36, 8 October 2012 Kn talk contribs uploaded File:Dektak 8 new position.JPG
- 15:48, 5 October 2012 Kn talk contribs uploaded File:Dektak XTA new.JPG (Dektak XTA)
- 13:21, 20 September 2012 Kn talk contribs uploaded File:Wafer plate.JPG (Wafer plate for PVD co-sputter/evaporation.)
- 14:54, 18 June 2012 Kn talk contribs uploaded File:III-V profiler.JPG (III-V profiler)
- 15:58, 15 June 2012 Kn talk contribs uploaded File:Physimeca.jpg (Physimeca)
- 15:41, 15 June 2012 Kn talk contribs uploaded File:P1040003.JPG (Chamber III-V dielectric evaporator)
- 15:40, 15 June 2012 Kn talk contribs uploaded File:IMG 3070.jpg (Picture of rack to the III-V Dielectric evap)
- 16:02, 5 January 2012 Kn talk contribs uploaded File:MWNT Kapar Haume.JPG (Example MWNT from Black Magic)
- 09:51, 4 January 2012 Kn talk contribs uploaded File:BM chamber.JPG (Open Black magic chamber)
- 10:29, 3 January 2012 Kn talk contribs uploaded File:Black magic PECVD.JPG
- 15:29, 25 October 2011 Kn talk contribs uploaded File:Schematic XPS.JPG
- 15:25, 25 October 2011 Kn talk contribs uploaded File:XPS electron levels.pdf
- 15:23, 25 October 2011 Kn talk contribs uploaded File:XPS electron levels.pptx
- 09:27, 24 October 2011 Kn talk contribs uploaded File:Si2p.JPG (XPS spectrum, Si2p (HF treated, not treated))
- 09:47, 18 October 2011 Kn talk contribs uploaded File:XPS instrument2.JPG (XPS instrument)
- 09:44, 18 October 2011 Kn talk contribs uploaded a new version of File:XPS instrument.JPG (XPS instrument)
- 09:42, 18 October 2011 Kn talk contribs uploaded File:XPS instrument.JPG (XPS instrument)
- 16:27, 17 October 2011 Kn talk contribs uploaded File:Overview spectra Labadvisor.JPG (Overview spectra XPS from a Si sample)
- 16:13, 17 October 2011 Kn talk contribs uploaded File:XPS technique.JPG (XPS)
- 16:02, 17 October 2011 Kn talk contribs uploaded File:Si spectra Labadvisor.JPG (XPS Si spectrum)
- 15:54, 17 October 2011 Kn talk contribs uploaded File:Si spectra Labadvisor.pdf (XPS spectra of SiO)