- 16:04, 17 February 2015 Paphol talk contribs uploaded File:Rs on 4in boron doped poly .png (Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour. Result from Trine H. Christensen DTU Space)