- 14:22, 7 April 2011 Jml talk contribs uploaded File:WF 2E05 mar23 2011-150b.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.32 recipe, Run ID 465, 466 and 467, time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/30 coil/platen, 50 degs. 100 mm spacers)