- 12:18, 12 January 2026 Jehem talk contribs created page Specific Process Knowledge/Lithography/Strip/plasmaAsher05 (Created page with "=Plasma Asher 5= 400px|thumb|Plasma asher 5 in cleanroom E-5.|right Product name: PVA Tepla Gigabatch 380M<br> Year of purchase: 2024 The Plasma Asher 5 can be used for the following processes: *Photoresist stripping *Descumming *Surface cleaning *Removal of organic passivation layers and masks Furthermore plasma processing using CF<sub>4</sub> in plasma asher 5 can be used for: *Etching of glass and ceramic *Etching of SiO<sub>2</sub>, Si<sub>3...")