- 11:50, 16 September 2025 Pevo talk contribs created page Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurementsn/A2 furnace break-down voltage measurement results (Created page with "==Breakdown voltage results for the A2 Gate Oxide furnace== ===Dry oxidation=== {| border="2" cellspacing="2" cellpadding="5" style="text-align: center;" |- |'''Date''' |'''Oxidation recipe''' |'''Oxide thickness''' |'''Absolute break-down voltage''' |'''Relative break-down voltage''' |- |'''February 2022''' |DRY1050 |150 nm |350x350px|thumb|left |image:2022-02-08_10-56-57_Wafer_A2_150nm_Rel.png|350x350px|thumb|le...")