  • 12:54, 29 August 2025 Prakus talk contribs created page Specific Process Knowledge/Etch/Titanium Nitride/ICP metal (Created page with " == Etching of Titanium nitride with resist as masking material - on 6" carrier wafer == This recipe was adapted from Evgeniy Shkondin recipe from 2018. This recipe is still under investigation. {| border="2" cellspacing="2" cellpadding="3" !Parameter !A Etch with carrier |- |Coil Power [W] |500 |- |Platen Power [W] |10 |- |Platen temperature [<sup>o</sup>C] |0 |- |Cl<sub>2</sub> flow [sccm] |5 |- |Ar flow [sccm] |5 |- |Pressure [mTorr] |10 |- |} {| border="2" cel...")