  • 18:13, 30 July 2025 Eves talk contribs created page Specific Process Knowledge/Thin film deposition/Deposition of NbTi (Created page with "=Niobium Nitride= Niobium–titanium (Nb‑Ti) is a ductile, readily machinable alloy that merges niobium’s superconductivity with titanium’s strength, yielding a rigid, corrosion‑resistant material valued in cryogenic and high‑field environments. Thin films are produced chiefly by magnetron sputtering, where the Nb/Ti ratio and post‑anneal determine phase purity, resistivity, and the superconducting critical temperature (≈ 9.2 K for near‑eutectic co...")