Combined display of all available logs of LabAdviser. You can narrow down the view by selecting a log type, the username (case-sensitive), or the affected page (also case-sensitive).
- 14:40, 30 July 2025 Eves talk contribs created page Specific Process Knowledge/Thin film deposition/Deposition of Tantalum/Sputtering of Ta in Sputter-System Metal-Nitride-PC3/Ta PC3 Src3 DC test 2022 (Created page with "<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br> All images and photos on this page belongs to <b>DTU Nanolab</b>.<br> The fabrication and characterization described below were conducted in <b>2022 by Evgeniy Shkondin, DTU Nanolab</b>.<br></i> <b>Important Note!</b> The deposition was carried out in 2022 with a weakened magnetron! This explains the high DC bias voltages. The magnetron was changed to an HSM type in 2024. For...")