- 14:35, 30 July 2025 Eves talk contribs created page Specific Process Knowledge/Thin film deposition/Deposition of Tantalum/Sputtering of Ta in Sputter-System Metal-Nitride-PC3 (Created page with "<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br> All images and photos on this page belongs to <b>DTU Nanolab</b>.<br> The fabrication and characterization described below were conducted in <b>2025 by Rawa Tanta</b> and <b>Evgeniy Shkondin, DTU Nanolab</b>.<br></i> =Ta DC Sputtering= This document presents the results of tantalum (<b>Ta</b>) deposition performed by DC sputtering in the <i>Metal-Nitride sputter system (PC3...")