- 19:16, 25 July 2025 Eves talk contribs created page Specific Process Knowledge/Thin film deposition/Deposition of Niobium Nitride/NbN Reactive Sputtering in Cluster Lesker PC3 (Created page with "<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br> All images and photos on this page belongs to <b>DTU Nanolab</b>.<br> The fabrication and characterization described below were conducted in <b>2025 by Evgeniy Shkondin, DTU Nanolab</b>.<br></i> The histogram experiment, where the DV bias voltage was measured as a function of N<sub>2</sub> flow for different Ar setpoints, was acquired together with <b>Sangeeth Kallatt</b> (san...")