- 12:17, 31 January 2023 Jehem talk contribs created page Specific Process Knowledge/Lithography/TIspray (Created page with "{{:Specific Process Knowledge/Lithography/authors_generic}} '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/5214E click here]''' Resist AZ 5214E __TOC__ =Resist Description= TI Spray is specifically designed to be used for spray coating, and is a positive UV photoresist with image revers...")