Polymer injection molding

The injection molder at Danchip is an Engel Victory Tech 80/45. It is hydraulic machine capable of up to 450 kN of clamping force.

The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:

 
Injection molding machine in the basement under the cleanroom

Polymer injection molding Info on LabManager

Process information

Equipment performance and process related parameters

Parameter Value
Sample dimensions Diameter

50, 100 or 150 mm (~ 2", 4" or 6")

Sample thickness

Maximum 1,0 mm

Process parameters Temperature

52*C

pH

3,5 - 3,8

Sample requirements Seed metal

100 nm of either NiV, Ti+Au or Cr+Au recommended. Most commonly seed metals are sputtered using the Sputter-System(Lesker).

Allowed materials

Most materials allowed. See below.

Forbidden materials

Copper, cobalt. See machine manual on LabManager for details