Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium Etch Metodes
| Cr wet etch 1 | Cr wet etch 2 | ICP metal | IBE (Ionfab300+) | |
|---|---|---|---|---|
| Generel description | Wet etch of pure Al | Wet etch of Al + 1.5% Si | Dry plasma etch of Al | Sputtering of Al - pure physical etch |
| Etch rate range |
|
|
|
|
| Etch profile |
|
|
|
|
| Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
|
|
|
|
Ething of Chromium can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done either with ICP using Chlorine chemistry or with IBE by sputtering with Ar ions.
Dry etching of chromium
On the ICP Metal Etch tool a recipe for chromium is being developed.