Etch of silicon can be done by either wet etch or dry etch. The standard setups for this here at DANCHIP are:
Wet etches:
Dry etches:
Comparison of KOH etch, wet PolySilicon etch, RIE etch, ASE etch and DRIE-Pegasus for etching of Silicon
|
KOH
|
PolySilicon etch
|
RIE
|
ASE
|
DRIE-Pegasus
|
General description
|
- Anisotropic etch in the (100)-plan
- High selectivity to the other plans
|
- Isotropic etch in Silicon and Polysilicon
|
- Can etch isotropic and anisotropic depending on the process parameters
- Anisotropic etch: vertical sidewalls independent of the crystal plans
|
- As RIE but better for high aspect ratio etching and deep etches (higher etch rate)
- Good selectivity to photoresist
|
- State-of-the-art dry silicon etcher with atmospheric cassette loader
- Extremely high etch rate and advanced processing options
|
Possible masking materials
|
- Silicon Nitride
- Silicon Oxide
|
|
- Photoresist
- E-beam resist
- Silicon Oxide
- Silicon Nitride
- Aluminium
- Chromium (ONLY RIE2!)
- Other metals if they cover less than 5% of the wafer area (ONLY RIE2!)
|
- Photoresist
- Silicon Oxide
- Silicon Nitride
- Aluminium
|
- Photoresist and zep resist
- Silicon Oxide
- Silicon Nitride
- Aluminium oxide
|
Etch rate
|
- Si(100) @80oC: 1.29+0.05 µm/min
- Si(100) @70oC: ~0.7 µm/min
- Si(100) @60oC: ~0.4 µm/min
|
- ~100-200 nm/min, highly dependent on doping level
|
- <40nm/min to >600nm/min depending on recipe parameters and mask design
|
- <130nm/min to >5.6 µm/min depending on recipe, mask design and aspect ratio.
|
- Up to 18-20 µm/min depending on recipe, mask design and aspect ratio.
|
Size of substrate
|
- 4" in our standard bath
- 4", 2" in "Fumehood KOH"
|
|
- 4" (or smaller with carrier)
|
- 6" (when it is set up for 6") and 4" (or smaller if you have a carrier)
|
- 6" (when it is set up for 6") and 4" (or smaller if you have a carrier)
|
Batch size
|
- 25 wafers at a time
- 1-5 wafers in "Fumehood KOH"
|
|
|
|
- One wafer at a time but you can load a whole batch of 25 wafers and set up an individual for each one
|
Allowed materials
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Other materials (only in "Fumehood KOH")
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
- Aluminium
- Chromium (ONLY RIE2!)
- Other metals if they cover less than 5% of the wafer area (ONLY RIE2!)
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
- Aluminium
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- zep resist
- Aluminium oxide
|
This Part is under construction
Feedback to this page: click here
Comparing silicon etch methodes at Danchip
There are a broad varity of lithography methodes at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs.
Comparison methode 1 and methode 2 for the process
|
Photolithography
|
DUV Lithography
|
E-beam Lithography
|
Imprint Lithography
|
Two photon polymerization Lithography
|
Generel description
|
Generel description - methode 1
|
Generel description - methode 2
|
3
|
4
|
5
|
Pattern size range
|
|
|
|
|
|
Resist type
|
|
|
- E-beam sensitive
- ZEP502A (positive)
- HSQ (negative)
- SU8
|
|
|
Resist thickness range
|
|
|
|
|
|
Typical exposure time
|
2s-30s pr. wafer
|
?-? pr. ?
|
?-? pr. µm2
|
? pr. wafer
|
? pr. µm2
|
Substrate size
|
- # small samples
- # 50 mm wafers
- # 100 mm wafers
- # 150 mm wafers
|
- # small samples
- # 50 mm wafers
- # 100 mm wafers
- # 150 mm wafers
|
We have cassettes that fit to
- # 4 small samples (20mm, 12mm, 8mm, 4mm)
- # 6 wafers of 50 mm in size
- # 2 wafers of 100 mm in size
- # 1 wafer of 150 mm in size
|
- # small samples
- # 50 mm wafers
- # 100 mm wafers
- # 150 mm wafers
|
- # small samples
- # 50 mm wafers
- # 100 mm wafers
- # 150 mm wafers
|
Allowed materials
|
- Allowed material 1
- Allowed material 2
|
- Allowed material 1
- Allowed material 2
- Allowed material 3
|
- Si, SiO2, III-V materials
|
- Allowed material 1
- Allowed material 2
- Allowed material 3
|
- Allowed material 1
- Allowed material 2
- Allowed material 3
|