Specific Process Knowledge/Thermal Process/C4 Aluminium Anneal furnace
Appearance
C4 Aluminium Anneal furnace
The C4 Aluminium Anneal furnace is a Tempress horizontal furnace for annealing of silicon wafers with aluminium.
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed to enter wafers that contains aluminium. Check the cross contamination chart.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
- Annealing: look at the Annealing page
| Purpose | Annealing | Annealing of wafers containing aluminium. |
|---|---|---|
| Performance | Film thickness | |
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
Silicon wafers with alluminium. Wafers are allowed after alluminium lift off or after alluminium etch and resiststrip in acetone |