Specific Process Knowledge/Etch/DRIE-Pegasus/StandardRecipes

From LabAdviser
Revision as of 11:54, 26 November 2012 by Jml (talk | contribs) (Created page with "== Overview of the standard processes: Processes A, B, C, D and SOI == The instrument was accepted on the basis of the performance of 5 processes. Below is a general compari...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Overview of the standard processes: Processes A, B, C, D and SOI

The instrument was accepted on the basis of the performance of 5 processes. Below is a general comparison - to find more detailed information, go the web page for each process

Standard processes on the DRIE-Pegasus
Process name Type Purpose Conditions during original runs Best usage
Feature Mask material Etch load Comments
Process A Bosch Fast etch 80 µm trench Photo resist 12-13 % on 6" wafer
Process B Bosch Fast etch 30 µm diameter via Photo resist 12-13 % on 6" wafer