Specific Process Knowledge/Characterization/Optical microscope
Appearance
| Zeiss Jenatech (strain) | Nikon SMZ 1500 | Leica S8 APO | Zeiss Original | Leitz Medilux | Zeiss Axiotron 2 | Zeiss Jenatech (particles measurements) | Noco IR microscope | Nikon SMZ 1000 | Nikon ME 600 | Nikon Eclipse L200 | Nokin Eclipse L200 (2) | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Location | Cleanroom 15 | Cleanroom 13 | Cleanroom 4 | Cleanroom 4 | Cleanroom 4 | Cleanroom Hymite | Cleanroom 2 | Cleanroom III-V | Cleanroom III-V | Cleanroom 4 | Cleanroom 13 | Cleanroom 3 |
| Special features | Nomarski prism | Stereoscopic microscope | Stereoscopic microscope | No | No | No | No | IR to visible | Stereoscopic microscope | No | Motorized stage | No |
| Ocular magnification | 10x | No | No | 10x | 10x | 10x | 10x | 10x | No | 10x | 10x | 10x |
| Objective magnification | 2.5x, 5x, 10x, 20x, 50x | Zoom 100x | Zoom 80x | 5x, 10x, 20x, 50x, 100x | 2.5x, 5x, 10x, 20x, 50x | 5x, 10x, 20x, 50x | 5x, 10x, 20x, 50x, 100x | 2.5x, 5x, 20x, 50x | Zoom 100x | 5x, 10x, 20x, 50x, 100x | 2.5x, 5x, 10x, 20x, 50x, 100x | 2.5x, 5x, 10x, 20x, 50x |
| Bright field | Yes | No | No | Yes | Yes | Yes | Yes | Yes | No | Yes | Yes | Yes |
| Dark field | Yes | No | No | Yes | No | Yes | Yes | No | No | Yes | Yes | Yes |
| Polarizer | Yes | No | No | Yes | No | No | Yes | No | NO | Yes | No | NO |
| Episcopic light (reflected light) | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes |
| Diascopic light (transmitted light) | No | Yes | No | No | Yes | Yes | No | Yes | No | No | Yes | Yes |
| View with eye | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes | Yes |
| View on screen (camera) | Yes | No | NO | Yes | Yes | Yes | No | Yes | No | Yes | Yes | Yes |
| Measurement option | No | No | No | No | NO | Yes | No | No | No | No | Yes | Yes |
| Zeiss (RR2) | Leica (RR3) | Leitz (RR4 Glassroom1) | Zeiss (RR4 Glassroom1) | Zeiss (RR4) | Nikon (K10 yellow room) | |
|---|---|---|---|---|---|---|
| Magnification | 25,50,100,
200,500x |
50,100,200,
500,1000x |
25,50,100,
200,500x |
50,100,200,
500,1000x |
25,50,100,
200,500x |
50,100,200,
500,1000x |
| Bright field | yes | yes | yes | yes | yes | yes |
| Dark field | yes | yes | yes | yes | yes | yes |
| Polarizer | yes | no | no | yes | yes | no |
| Episcopic light (reflected light) | yes | yes | yes | yes | yes | yes |
| Diascopic light (transmitted light) | no | yes | yes | no | no | yes |
| View with eye | yes | yes | yes | yes | yes | yes |
| View on screen | no | yes | yes | yes | no | yes |
| Measurement option | no | no | yes | yes | no | yes |