Specific Process Knowledge/Thermal Process/C1 Furnace Anneal-oxide
Appearance
C1 Furnace Anneal Oxide
C1 Furnace Anneal Oxide is a Tempress horizontal furnace for oxidation and annealing of silicon wafers.
This furnace is the second furnace tube in the furnace C-stack positioned in cleanroom 2. The furnaces are the cleanest process chambers in the cleanroom. In this furnace it is allowed to enter wafers that comes directly from PECVD1 (assuming they were very clean when entering PECVD1). Check the cross contamination chart. If you are in doubt, please ask one from the furnace team.
Process knowledge
| Purpose | Oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|