Nickel deposition
Nickel can be deposited by e-beam evaporation or sputtering at DTU Nanolab. For electroplating you will have to contact other institutes at DTU, e.g., DTU Mechanical Engineering.
Some process information is available here for e-beam evaporated films:
In the chart below you can compare the different deposition equipment:
E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | Sputter deposition (Lesker) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | |
---|---|---|---|---|
General description | E-beam deposition of Nickel | E-beam deposition of Nickel | Sputter deposition of Nickel | Sputter deposition of Nickel |
Pre-clean | Ar ion bombardment | RF Ar clean | RF Ar clean | |
Layer thickness | 10 Å to 1 µm * | 10 Å to 1 µm * | 10 Å to 5000 Å ** | 10 Å to 5000 Å ** |
Deposition rate | 2-10 Å/s | 10-15 Å/s | Depends on process parameters, about 1 Å/s | Depends on process parameters, at least ~ 4 Å/s, see conditions here |
Batch size |
|
|
|
|
Allowed materials |
|
|
|
|
Comment |
|
|
* To deposit a cumulative thickness above 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
** To deposit a cumulative thickness above 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
Quality control of e-beam evaporated Ni films
Quality control (QC) for Wordentec | ||||||||||||||||
Thickness is measured in 5 points with a stylus profiler. |
Quality control (QC) for the Temescal | ||||||||||||||||||
Thickness is measured in 5 points with a stylus profiler. |