Etching of nanostructures in silicon using the ICP Metal Etcher
| Sinano3.0 | Sinano3.1 | Sinano3.2 | Sinano3.3 | Sinano3.4 | Sinano4.0 | Sinano3.5 | Sinano3.6 | |
|---|---|---|---|---|---|---|---|---|
| Cl2 | 0 | 0 | 0 | 0 | 0 | 20 | 15 | 15 |
| BCl3 | 5 | 3 | 5 | 5 | 5 | 0 | 5 | 5 |
| HBr | 15 | 17 | 15 | 15 | 15 | 0 | 0 | 0 |