Specific Process Knowledge/Back-end processing/Polymer Injection Molder
The injection molding machine is located in the basement of building 346 (room 904). The machine can be booked from LabManager (not active yet).
The following polymers are presently available:
Polystyrene Basell Lupolen
Topas (COC from Ticona) 5013S-04 6015S-04 6017S-04 8007S-04
Other polymers (PE, PBT, PCT, PC, POM, PP, PU, SAN) are available in smaller amounts. Ask Danchip for details (choi@danchip.dtu.dk).