Specific Process Knowledge/Etch/Aluminum Oxide/Al2O3 Etch with ICP Metal
Jump to navigation
Jump to search
Feedback to this page: click here
Al2O3 etching with the ICP metal
Al2O3 etching by sanvis@nanolab
Parameter | Recipe name: no name (testing recipe) |
---|---|
Coil Power [W] | 1200 |
Platen Power [W] | 200 |
Platen temperature [oC] | 0 |
BCl3 flow [sccm] | 60 |
Cl2 flow [sccm] | 30 |
Pressure [mTorr] | 4 |
Material to be etched | Etch rate using the above parameters |
---|---|
Al2O3 |
|