Deposition of TiW alloy can be done in the Wordentec. If necessary, processes may also be developed for depositing TiW in the Lesker sputter setups (contact responsible staff for this).


Sputtering of TiW


Sputter deposition (Wordentec)
General description Sputter deposition of TiW
Pre-clean RF Ar clean
Layer thickness .
Deposition rate Depending on process parameters, see here.
Batch size
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Allowed substrates
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
Allowed materials
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Comments TiW alloy: 10%/90% by weight


Deposited film characteristics

AFM pictures show how the surface roughness is dependent on the process parameters.

For the sputter process, the effect and argon pressure can be set to different values. Depending on the process parameters, the deposited layers will have different characteristics: the roughness, grain size and uniformity may be differnt.


Effect 150 W, pressure 1*10-3 mbar

With use of the settings 150W and 1*10-3 mbar, a surface with low roughness is deposited.

 
AFM picture of sputter deposited TiW. Used settings: 150W and 1*10-3 mbar.


Measurement done September 2008, KNIL.