Specific Process Knowledge/Thin film deposition/Temescal/Acceptance Test
< Specific Process Knowledge | Thin film deposition | Temescal
Jump to navigation
Jump to search
Revision as of 16:26, 12 September 2018 by Reet (talk | contribs) (→Acceptance test and test results)
Feedback to this page: click here
Acceptance test and test results
In the acceptance test, we tested the vacuum performance, the ion source, and the uniformity of the deposited metal films.
The uniformity of the ion beam etch was tested on Si wafers with SiO2 coating of a known thickness.
For metal films, the thickness and for Ti/Ni the sheet resistance uniformity were measured.
Side wall coverage was evaluated in SEM for Ti/Au films deposited at normal incidence (what most users require, which gives no side-wall deposition) and with various degrees of tilt.
Full acceptance test report here:
File:Temescal Acceptance Test Results Mar-April-May 2018.pdf