Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/ProcessD/PrD-4

From LabAdviser
Revision as of 17:11, 19 January 2015 by Jmli (talk | contribs) (Created page with " {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" |+ '''Process runs''' |- ! rowspan="2" width="40"| Date ! colspan="4" width="120"| Substrate Informat...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
8/1-2015 4" Wafer with travkaXX mask AZ standard Si / XX % Pegasus/jmli s004781 danchip/jml/showerhead/prD/PrD-4, 150 cyc or 8:00 mins S004782 New showerhead