Jump to content

Specific Process Knowledge/Back-end processing/Polymer Injection Molder

From LabAdviser

Feedback to this page: click here

Polymer injection molding

 
Injection molding machine in the basement under the cleanroom

The injection molder at Danchip is an Engel Victory Tech 80/45. It is a hydraulic machine capable of up to 450 kN of clamping force.


The user manual, user APV, technical information and contact information can be found in LabManager:

Polymer injection molding Info on LabManager

Process information

There are no standard processes on the injection molder, since the type of process chosen and process parameters will depend on which polymer that will be used and what type of pattern that is to be replicated during the molding process. At Danchip the following polymers are used routinely:

Topas 5013L-10
Topas 8007S-04
PP
PMMA

Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the request form found in LabManager here.

Equipment performance and process related parameters

Parameter Value
Processing temperatures Mold

Up to 160*C

Barrel

Absolute max: 350*C

Processing temperatures Temperature

Up to 160*C

Barrel

Absolute max: 350*C

Molding parameters Injection speed

Up to 53 cm3/s

Injection pressure

Up to 2200 bar

Switch-over point

Time, pressure, volumen or external signal