Recipe | Step | Temp. | Deposition step | Etch step | Process observations | |||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Time | Pres. | C4F8 | SF6 | O2 | Coil | Time | Pres. | C4F8 | SF6 | O2 | Coil | Platen | HW | Runs | Key words | |||
mediumiso1 | - | 20 | NA | NA | NA | NA | NA | NA | NA | 25 | 0 | 150 | 0 | 600 | 3 | - | 1 | NA |
- |
Recipe | Step | Temperature | Time | Pressure | C4F8 | SF6 | O2 | Ar | Coil | Platen | Runs | Key words |
---|---|---|---|---|---|---|---|---|---|---|---|---|
mediumiso1 | - | 20 | NA | 25 | 0 | 150 | 0 | 0 | 600 | 3 | 1 | NA |
- |