Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Lasers sources
Appearance
Laser sources
The laser micromachining tool is equipped with two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specification provided by the supplier 3D micromac are shown below. Refer to the Performances to know the measured values.
Specifications from 3D micromac
| Picosecond (TBW) | Nanosecond (IPG) | |
| Wavelength | 1064nm, 532nm, 355nm | 1064nm |
| Pulse duration | 10ps | 120ns |
| Repetition rate | 200 kHz up to 8000 kHz software controlled | 200kHz |
| Output power | > 50 W @ 1064 nm | 100 W |
| Warm-up time | 25min | none |