Feedback to this page: click here
Annealing
At Danchip we have three furnaces and an RTP (Rapid thermal annealing) that can be used annealing: C1, C3, Noble furnace and Jipelec RTP. Annealing normally takes place in an N2 atmosphere. PECVD PBSG glass is annealed in a wet atmosphere which will also oxidize the silicon substrate.
The recipes for oxidation are made so that a 20 minutes N2 annealing step is included after the oxiation step.
Comparison of the annealing furnaces
|
|
C1: Anneal Oxide
|
C3: Anneal Bond
|
Noble furnace
|
Jipelec RTP
|
Multipurpose Anneal Furnace
|
| General description
|
Annealing of 4" and 6" wafers. Annealing of wafers from the LPCVD furnaces and PECVD2.
|
Annealing of wafers from EVG-NIL, PECVD3 and wafers with aluminum.
|
Annealing of almost all materials on silicon wafers.
|
Rapid thermal annealing
|
Annealing, oxidation and resist pyrolysis of different samples
|
| Annealing gas
|
|
- N2
- Ar
- Wet annealing with bobbler (water steam + N2)
|
|
|
|
| Process temperature
|
|
|
|
- 20 oC - 1000 oC
- Ramp up to 300 C/min
|
- Vacuum: *20 oC - 1050 oC¨
- No vacuum: *20 oC - 1100 oC
|
| Substrate and Batch size
|
- Small samples on a carrier wafer, horizontal
- 1-30 50 mm wafers
- 1-30 100 mm wafers
- 1-30 150 mm wafers
|
- Small samples on a carrier wafer, horizontal
- 1-30 50 mm wafers
- 1-30 100 mm wafers
|
- Small samples on a carrier wafer, horizontal
- 1-25 50 mm wafers
- 1-25 100 mm wafers, vertical and horizontal
|
- Small samples on a carrier wafer, horizontal
- One 100 mm wafers on a carrier wafer
|
- 1-30 50 mm, 100 mm or 150 mm wafers per run
- 1-50 200 mm wafers per run
- Smaller samples (placed in a Si carrier wafer)
|
| Allowed materials
|
- All processed wafers have to be RCA cleaned, except wafers from LPCVD furnaces and PECVD1.
|
- All processed wafers have to be RCA cleaned, except wafers from EVG-NIL, PECVD3 and wafers for annealing of aluminum.
|
- Almost all materials, permission is needed.
|
- III-V samples
- Silicon wafers
- Some metals
|
- Depends on the furnace quartz ware:
- Clean: Samples that have been RCA cleaned
- Metal: Almost all materials, permission is needed
- Resist Pyrolysis
|