Revision as of 11:19, 26 June 2015 by Lynhen (talk | contribs) (While electroplating in the 0-degree tilt position, air bubbles were caught in the system and were not able to escape.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (861 × 661 pixels, file size: 154 KB, MIME type: image/jpeg)

While electroplating in the 0-degree tilt position, air bubbles were caught in the system and were not able to escape.