Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBE blazed gratings
Appearance
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
- Blazed gratingen in fused silica etched with Cr and DUV resist as masking layer
-
30min etch with 100nm Cr mask, used recipe BGHE blazed gratings with CHF3
-
45min etch with 100nm Cr mask, used recipe BGHE blazed gratings with CHF3
-
20min etch with Krf resist, all resist is gone, used recipe BGHE blazed gratings
-
15+30min etch with 50nm Cr mask, used recipe BGHE blazed gratings with CHF3