Specific Process Knowledge/Wafer cleaning
< Specific Process Knowledge
Jump to navigation
Jump to search
Revision as of 12:06, 11 February 2008 by 192.38.87.73 (talk)
Clean with:
- RCA - Two step process to remove organics and metals
- 7-up - Fake piranha etch of wafers and masks - removes organics and alkali ions
- Piranha - Removes organics and alkali ions
- 5% HF - Removing native oxide, etching of predep glass etc.
- IMEC - Cleaning before fusion bonding
- Soap Sonic - Cleaning of "dirty" wafers when entering the cleanroom