Specific Process Knowledge/Thin film deposition/Deposition of Palladium
Feedback to this page: click here
Palladium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | |
---|---|
General description | E-beam deposition of Pd |
Pre-clean | RF Ar clean |
Layer thickness | 10Å to 1µm* |
Deposition rate | 2Å/s to 10Å/s |
Batch size |
|
Allowed materials |
|
Comment |
* For thicknesses above 200 nm permission is requested.