The SPTS III/V ICP in the Danchip cleanroom B-1

The III-V ICP

The III-V ICP is a state-of-the-art etch tool. The combination of advanced hardware and software enables you to either use the optimized standard processes or to tailor etch processes for your specific needs. The tool can be used for etching of different materials, but is primarily intented for etching of III-V materials.

The user manual, user APV and contact information can be found in LabManager:

Equipment info in LabManager

Process information

Etch recipes

An overview of the performance of the III-V ICP and some process related parameters

Purpose Dry etch of
  • III-V materials such as GaAs, InP, GaN, AlGaAs, InGaAs or InGaAsP
  • Other materials such as Si, SiO2 or polymers on samples with III-V materials
Performance Etch rates
  • InP: ~500 nm/min (depending on features size and etch load)
  • GaAs : 5-500 nm/min (depending on etch process, features size and etch load)
  • GaN: ~500 nm/min (depending on features size and etch load)
Anisotropy
  • Good
Process parameter range Process pressure
  • ~0.1-100 mTorr
RF Generators
  • Coil power 1.5 kW
  • Platen power 600 W
Chiller temperature
  • Range 0-180 degrees
Gas flows
N2: 0-100 sccm Ar: 0-100 sccm
SF6: 0-100 sccm O2: 0-100 sccm
CF4: 0-100 sccm H2: 0-100 sccm
CH4: 0-100 sccm BCl3: 0-100 sccm
Cl2: 0-100 sccm HBr: 0-100 sccm
Substrates Batch size
  • 1 4" wafer per run
  • 1 2" wafer per run
  • Or several smaller pieces on a carrier wafer with recess
Substrate material allowed
  • III-V wafers
  • Silicon wafers
    • with layers of silicon oxide or silicon (oxy)nitride
  • Quartz wafers
Possible masking material
  • Photoresist
  • E-beam resist
  • DUV resist