Nickel Vanadium can be deposited by sputter evaporation. In the chart below you can compare the different deposition equipment.
Sputter deposition (PVD co-sputter/evaporation) | Sputter deposition (Sputter-System Lesker) | |
---|---|---|
General description | Sputter deposition of NiV | Sputter deposition of NiV |
Pre-clean | RF Ar clean | RF Ar clean |
Layer thickness | About 10Å to 4000Å | About 10Å to 5000Å |
Deposition rate | Depending on process parameters. | Depending on process parameters. |
Batch size |
|
|
Allowed substrates |
|
|
Allowed materials |
|
|
Comment | Sputter target with NiV composition: Ni/V 93/7% | Sputter target with NiV composition: Ni/V 93/7% |