Spin Coat of AllResist SX 6200/2, TIGRE, 09-04-2014 | ||
---|---|---|
Spin Coater | Process Parameters | Comments |
Spin Coater Manual, LabSpin, A-5 | 60 sec at various spin speed. Acceleration 4000 s-2, softbake 5 min at 150 deg Celcius | Resist poured directly from bottle |
AllResist SX 6200/2 spinning on Manual Spinner LabSpin A-5, TIGRE, 09-04-2014 | ||||||
---|---|---|---|---|---|---|
Spin Speed [rpm] | Acceleration [1/s2] | Spin Time [s] | Thickness [nm] | St Dev | ||
2000 | 4000 | 60 | ||||
3000 | 4000 | 60 | ||||
4000 | 4000 | 60 | ||||
5000 | 4000 | 60 | ||||
6000 | 4000 | 60 | ||||
7000 | 4000 | 60 |